south africa chromite sand price

south africa chromite sand price

/MT

south africa chromite sand

Foundry chromite sand is a natural process products of chromite through the broken screen classification, chrome ore, its main chemical composition of cr2o3, this kind of sand heated volume stability, high thermal conductivity, when in contact information with the molten metal, not only has good resistance to basic slag, not with ferric oxide and other chemical reactions, and itself has the characteristics of the solid phase sintering, can be a very good prevent the infiltration of molten metal, avoid to touch sand defects, suitable for all kinds of stainless steel, alloy steel and carbon steel gradually shape the original sand core and coating.

Foundry south africa 46% chromite sand AFS45-50

Item

Index

Cr2O3

≥46.0%

SiO2

≤1.0%

FeO

≤26.5%

CaO

≤0.30%

MgO

≤10.0%

Al2O3

≤15.5%

P

≤0.003%

S

≤0.003%

Cr/Fe

1.55:1

Bulk Density

2.5-3

Color

Black

PH

7-9

The amount of the acid

≤ 2 ML

Percent soil

≤0.1%

Percent Moisture

≤0.1%

The sintered

1600℃

Percentage of free acid present in the sand

0

filling density

 2.6g/cm³

sintering point

> 1800°C

melting temperature

 2180°C

Avaliable sizes

AFS25-35 AFS30-35 AFS35-40 AFS40-45 AFS45-55 AFS50-55 AFS55-60 AFS60-65 AFS60-70

Packing 1: 1mt big bag with 4 handles and top spout

Packing 2:1mt big bag with 4 handles,top spout and buttom spout.

Packing 3:1mt big bag with 2 handles and top spout

 

Foundry south africa 46% chromite sand AFS45-50Foundry south africa 46% chromite sand AFS45-50Foundry south africa 46% chromite sand AFS45-50

PDF-LOGO-100-.png

TDS not uploaded

PDF-LOGO-100-.png

MSDS not uploaded

Scroll to Top