Physical properties of South Africa Chromite Sand
South Africa Chromite Sand
Cr:Fe:1.6:1
Cr2O3:46%min
SiO2:1%max
Melting point of 2150°C.
Good thermal conductivity.
Good resistance to thermal shock.
Excellent resistance to metal penetration or burn-on.
Resists slag attack.
High dimensional stability.