particle size distribution of chromite sand AFS45-55
Chromite sand is suitable for various casting processes of stainless steel, alloy steel and carbon steel, such as sand casting, shell casting, lost foam casting, etc. In these processes, chromium ore sand can play an excellent role and ensure the quality and precision of castings.
chromite sand origin:south africa
size:AFS40-45 AFS45-50 AFS45-55 AFS50-55
particle size distribution of chromite sand AFS45-55
| Sieve | Micron | Mass-gram | Factor | Value |
| A | B | AXB | ||
| 6 | 3350 | 0 | 3 | 0 |
| 12 | 1400 | 0 | 5 | 0 |
| 20 | 850 | 0.02 | 10 | 0.2 |
| 30 | 600 | 2.3 | 20 | 46 |
| 40 | 425 | 6.84 | 30 | 205.2 |
| 50 | 300 | 35.52 | 40 | 1420.8 |
| 70 | 212 | 37.29 | 50 | 1864.5 |
| 100 | 150 | 14.56 | 70 | 1019.2 |
| 140 | 106 | 2.86 | 100 | 286 |
| 200 | 75 | 0.51 | 140 | 71.4 |
| 270 | 53 | 0.08 | 200 | 16 |
| -270 | -53 | 0.02 | 300 | 6 |
| 100 | 4935.3 | |||
| AFS49.35 | ||||