Analyze the casting defects such as shrinkage, porosity, cracks and surface sticky sand in the production of pump valve steel castings, and combine the material, structure and distribution of hot spots to try to replace chromite sand in actual production. Improve and achieve better results.Analyze the casting defects such as shrinkage, porosity, cracks and surface sticky sand in the production of pump valve steel castings, and combine the material, structure and distribution of hot spots to try to replace chromite sand in actual production. Improve and achieve better results.