Application of chromium ore powder in pigments:
Glass pigment: Chrome ore powder is mainly used in the glass industry for green coloring instead of red, destroying glass products to provide long-lasting green tones, such as emerald green, Georgia green, etc. It is widely used in beer, wine and other food packaging to resist aging and prolong life. Lifespan product shelf life.
Ceramic glaze: In the ceramic industry, chromite flour powder is used as a green glaze additive to produce ceramic products that require green coloring, but is not used for red ceramic glazes.
Other applications: chromite flour powder is also used in the manufacture of refractory materials, wear-resistant coatings and other fields. In these applications, physical properties such as fire resistance and wear resistance are more important than color properties.
In general, chromite flour is mainly use in green colorant in the glass and ceramic industries and other fields.
The most commonly used chromite flour powder siz are:
200# 325 400 600 800 1000 1200 1500 2000 2500 3000