Chromite Powder /chromite flour for Glass Bottle Pigment

Chromite Powder /chromite flour for Glass Bottle Pigment

Chromite powder (South Africa Chromite Flour) is the most commonly used and cost-effective mineral colorant for producing green and amber glass bottles. It mainly relies on chromium trioxide (Cr₂O₃) for coloration.

I. Core Properties of Chromite Powder/chromite flour

  • Main component: Cr₂O₃ ≥ 46%
  • Common particle sizes for glass bottle production: 200 mesh, 325 mesh, 400 mesh (325 mesh is the most widely used, 0–45 μm)
  • Maximum service temperature: Melting point approx. 2150℃, resistant to high-temperature glass melting at 1400–1600℃
  • Stability: Chemically stable, lightfast, weather-resistant, and UV-resistant
  • Cost advantage: More economical than synthetic chromium oxide pigments

II. Functions & Effects in Glass Bottles

  • Primary coloration: Emerald green, olive green, Georgian green, dark green, etc.
  • Auxiliary color matching: When combined with iron, manganese, etc., it can produce amber, brown glass bottles
  • Functional benefits: Blocks ultraviolet rays and extends the shelf life of beer, red wine and other beverages
  • Applications: Beer bottles, wine bottles, beverage bottles, food packaging bottles, decorative glass bottles

III. Application Guidelines

  • Addition method: Added directly to the glass batch and mixed evenly before melting
  • Dosage control: Generally 0.5%–3% (adjusted according to the desired color depth)
  • Selection for green and amber glass ottles:
    • 200/325 mesh: For general-purpose green bottles with high cost performance
    • Above 400 mesh: Finer texture and more uniform color, suitable for high-quality bottles
Note: As a natural mineral, chromite powder may have slight color differences between batches, requiring stable raw materials and formulations.

IV. Comparison between Chromite Powder & Synthetic Chromium Oxide

ItemNatural Chromite PowderSynthetic Chromium Oxide (Cr₂O₃)
CostLowHigh
Color ToneOlive green, natural greenPure, bright emerald green
High-Temperature StabilityExcellentExcellent
ImpuritiesContains small amounts of iron, magnesium, etc.High purity
ApplicationsGeneral-purpose green / amber bottlesHigh-end bottles requiring high color purity

V. Selection & Purchasing Recommendations

  • Prioritize South African chromite powder with Cr₂O₃ ≥ 46%, 325 mesh, and uniform particle size
  • Require suppliers to provide chemical composition, particle size distribution, and fired color samples, and conduct small-scale tests to confirm performance
  • Suitable for mass production of glass bottles with cost sensitivity and demand for natural green tones