Content requirements of SiO2 in chromite sand?
South African chromite sands all require the content of SiO2 to be less than 1%. If it exceeds 1%, then this batch of chromite sands is an unqualified product.
Content requirements of SiO2 in chromite sand?
South African chromite sands all require the content of SiO2 to be less than 1%. If it exceeds 1%, then this batch of chromite sands is an unqualified product.