Moisture of south africa chromite sand
our chromite sand origin:south africa
cr2o3 content:46%min
SiO2 content:1%max
Moisture of south africa chromite sand:≤0.2%
Moisture of south africa chromite sand
our chromite sand origin:south africa
cr2o3 content:46%min
SiO2 content:1%max
Moisture of south africa chromite sand:≤0.2%