Chromite ore is mined in over 20 countries, but about 80% of production originates from four countries: South Africa, India, Kazakhstan, and Turkey

Our chormite sand origin:south africa,We import from South Africa and then screen it in Lianyungang

chromite sand size:AFS20-25 AFS25-30 AFS30-35 AFS35-40 AFS40-45 AFS45-50 AFS50-55