particle size distribution of chromite sand AFS45-55

particle size distribution of chromite sand AFS45-55

Chromite sand is suitable for various casting processes of stainless steel, alloy steel and carbon steel, such as sand casting, shell casting, lost foam casting, etc. In these processes, chromium ore sand can play an excellent role and ensure the quality and precision of castings.

chromite sand origin:south africa

size:AFS40-45 AFS45-50 AFS45-55 AFS50-55

particle size distribution of chromite sand AFS45-55

SieveMicronMass-gramFactorValue
ABAXB
63350030
121400050
208500.02100.2
306002.32046
404256.8430205.2
5030035.52401420.8
7021237.29501864.5
10015014.56701019.2
1401062.86100286
200750.5114071.4
270530.0820016
-270-530.023006
1004935.3
AFS49.35