Chromite sand introduction
Casting Grade Chromite Sand For Foundry Price
The chromite sand is a product of south africa natural chromite ore after crushing and sieving, and its main chemical composition is Cr2O3.
*Melting point of 2150°C
*Good thermal conductivity
*Good resistance to thermal shock
*Excellent resistance to metal penetration or burn-on
*Resists slag attack
*High dimensional stability
Chromite sand physical and chemical index
Item | Index |
Cr2O3 | ≥46.0% |
SiO2 | ≤1.0% |
FeO | ≤26.5% |
CaO | ≤0.30% |
MgO | ≤10.0% |
Al2O3 | ≤15.5% |
P | ≤0.003% |
S | ≤0.003% |
Cr/Fe | 1.55:1 |
Bulk Density | 2.5-3g/cm³ |
Color | Black |
PH | 7-9 |
The amount of the acid | ≤ 2 ML |
Percent soil | ≤0.1% |
Percent Moisture | ≤0.1% |
The sintered | 1600℃ |
Percentage of free acid present in the sand | 0% |
filling density | 2.6g/cm³ |
sintering point | > 1800°C |
melting temperature | 2180 °C |
Chromite sand application
*Chromite Sand in the steel industry
*Chromite Sand in the foundry industry