Chromite sand/chromite flour 0-0.1mm

Chromite sand / chromite flour 0–0.1mm is an ultra-fine powder produced by crushing, grinding and classifying natural chromite. Its main component is FeO·Cr₂O₄. It is blackish-brown, featuring high refractoriness, high density and chemical inertness.

/MT

chromite Sand / Chromite Flour 0–0.1mm

Chromite sand / chromite flour 0–0.1mm is an ultra-fine powder produced by crushing, grinding and classifying natural chromite. Its main component is FeO·Cr₂O₄. 

 Key Specifications (0–0.1mm)

  • Particle size: 0–100 μm, commonly corresponding to mesh sizes: 200 mesh (≤75 μm), 325 mesh (≤45 μm), 
  • Main ChemicalCr2O3·FeO
    Hardness:Mohs:5.5-6
    Melting Point:Sublimes at 2180 ℃
    Sintering point:>1800℃
    Color:Dark brown/ Dark red black
    PH7-9
    Percentage of Moisture≤0.1
    CAS No.:1308-31-2
  • ItemGuarantee ValueTypical Value
    Cr2O3≥46.0%46.36%
    SiO2≤1.0%0.94%
    FeO+Fe2O326-28%27.01%
    AL2O3≤15.5%13.62%
    TiO2≤1.0%0.63%
    CaO≤0.3%0.12%
    MgO≤10%9.35%
    Na2O≤0.5%0.12%
    MnO≤0.5%0.32%
    ZnO≤0.2%0.09%
    NiO≤0.2%0.11%
    P≤0.003%/
    S≤0.003%/