South Africa Chromite Sand

The chromite sand casting is compatible with all chemical processes of agglomeration of moulds and cores. Currently used large amounts of chromite sand in the foundry industry for the manufacture of moulds and cores. Chromite Sand is applicable to all types of steels and very appropriate for chrome steel, chrome-nickel and manganese steel. Has the advantage over silica sand that is less reactive with manganese oxide, reducing the problems of ignition and metal-mould reactions

$330.00 – $550.00 / MT

Origin:south africa

south africa chromite sand chemical -physical index

ItemIndex
Cr2O3≥46.0%
SiO2≤1.0%
FeO≤26.5%
CaO≤0.30%
MgO≤10.0%
Al2O3≤15.5%
P≤0.003%
S≤0.003%
Cr/Fe1.55:1
Bulk Density2.5-3
ColorBlack
PH7-9
The amount of the acid≤ 2 ML
Percent soil≤0.1%
Percent Moisture≤0.1%
The sintered1600℃
Percentage of free acid present in the sand0
filling density 2.6g/cm³
sintering point> 1800°C
melting temperature 2180°C
Avaliable sizes
AFS25-35 AFS30-35 AFS35-40 AFS40-45 AFS45-50 AFS45-55 AFS50-55 AFS55-60 AFS60-65 AFS60-70