Which size chromite flour suitable for producing green glass bottles?
Common applicable models
producing green glass bottles available size ofchromite flour :200 mesh, 325 mesh and 400 mesh ,it can replace chromium green as pigment.
Features of different types of chromite powder
325 mesh chromite powder
Size: Its size is 45um – 0.
Production process: Grind it once in a ball mill.
Difficulty of obtaining: This chromite powder is easy to obtain.
Pass rate: The pass rate of chromite powder 325# – 0 screen is 95%, 97% and other specifications.
400 mesh chromite powder
Size: The size is 38um – 0.
Production process: It must be ground twice to obtain finer particles.
Difficulty of obtaining: Customized production is required.
Advantages: Higher grade, stricter particle size control, can reduce the cost of green glass products, and reduce the pollution of chemical colorants.