South africa chromite sand for casting

South africa chromite sand for casting

/MT

South africa chromite sand for casting AFS40-45 AFS45-50 AFS 50-55 AFS55-60 AFS55-65
South africa chromite sand is a product of south africa natural chromite ore after crushing and sieving, and its main chemical composition is Cr2O3.
chromite sand for foundry packing:1mt big bag
South africa chromite sand physical-chemical
Item
Index
Cr2O3
≥46.0%
SiO2
≤1.0%
FeO
≤26.5%
CaO
≤0.30%
MgO
≤10.0%
Al2O3
≤15.5%
P
≤0.003%
S
≤0.003%
Cr/Fe
1.55:1
Bulk Density
2.5-3
Color
Black
PH
7-9
The amount of the acid
≤ 2 ML
Percent soil
≤0.1
Percent Moisture
≤0.1
The sintered
1600
Percentage of free acid present in the sand
0
filling density
2.6
sintering point
> 1,800
melting temperature
2,180