Chromite sand foundry

Foundry chromite sand is a natural process products of chromite through the broken screen classification, chrome ore, its main chemical composition of cr2o3, this kind of sand heated volume stability, high thermal conductivity, when in contact information with the molten metal, not only has good resistance to basic slag, not with ferric oxide and other chemical reactions, and itself has the characteristics of the solid phase sintering, can be a very good prevent the infiltration of molten metal, avoid to touch sand defects, suitable for all kinds of stainless steel, alloy steel and carbon steel gradually shape the original sand core and coating.

$400.00 – $550.00 / MT

chromite sand chemical-physical properties

temIndex
Cr2O3≥46.0%
SiO2≤1.0%
FeO≤26.5%
CaO≤0.30%
MgO≤10.0%
Al2O3≤15.5%
P≤0.003%
S≤0.003%
Cr/Fe1.55:1
Bulk Density2.5-3
ColorBlack
PH7-9
The amount of the acid≤ 2 ML
Percent soil≤0.1%
Percent Moisture≤0.1%
The sintered1600℃
Percentage of free acid present in the sand0
filling density2.6g/cm³
sintering point> 1800°C
melting temperature2180°C

Chrome ore USES For drainage sand materials, casting, ceramic, glass and refractory, etc.

Chromite sand applicable types: 1) casting grade is special      2)special metallurgy level.

(1)Chrome ore in casting production is mainly used for large steel surface sand, prevent casting surface adhering sand;

(2)Secondly the grinding powder for the refractory aggregate of foundry coating, chrome ore is chilling material, when modelling (core) alternative part cold iron.

Chromite sand for casting coating, refractory materials, brake pads, high-performance ceramic materials, ceramic and glass colorant, friction material, chemical and metallurgical casting, etc.

PDF-LOGO-100-.png

TDS not uploaded

PDF-LOGO-100-.png

MSDS not uploaded

Scroll to Top