chromite sand 325mesh 400mesh for glass pigment
Chromite flour use as colorant in glass bottle fields. Originally from South Africa. The sand is produced by crushing chrome ore and its washing in spiral concentrators, subsequent drying, dust cleaning, screening and sorting as per grain size.The fine size is grinded to different powder such as 200mesh 325mesh 400mesh etc


Product Parameters
CHEMICAL | PHYSICAL | ||
Cr2O3 | 46.0%min | Bulk Density | 2.5-3g/cm3 |
SiO2 | 1.0%max | PH Value | 7-9 |
FeO | 26.5%max | The amount of the acid | 2ML max |
CaO | 0.3%max | Percent soil | 0.1%max |
MgO | 10.0%max | Percent Moisture | 0.1%max |
Al2O3 | 15.5%max | The sintered | 1600℃ |
P | 0.003%max | Specific Gravity | 4.0-4.8g/cm3 |
S | 0.003%max | Filling Density | 2.6g/cm3 |
Cr/Fe | 1.55/1 | melting temperature | 2180°C |
MAIN APPLICATIONS
Chromite Sand in the foundry industry
Its properties enable the material to be used in high duty grey iron and steel foundries as core and mould making sand. Its high thermal conductivity gives it good chilling properties, low thermal expansion gives rise to good dimensional stability. Its basicity being close to neutral allows the use of a wide range of resin bonding systems and inorganic binders, it has a high refractoriness and a broad sieve distribution.
Chromite Sand in the steel industry
In steel production, Chromite Sand is used as well filler for protection of the sliding gate in large steel holding ladles.
Chromite Sand in the glass industry
When ground to a fine flour, Chromite Sand is used for the production of green glass beverage containers.
OUR FACTORY

Raw Material
Wash chrome ore

Conveyor
Put the chrome ore into stock bin then convey to drying oven

Drying plant
Fuel—bio-particles

Magnetic separation and Screening
the macrogrits will be sorted to different sizes such as AFS25-30 AFS30-35 AFS435-40 AFS40-45 AFA45-50 etc and the fine will be separated and conveyed to grinding mill

Grinding mill
The fine size will be grinded in the mill to different sizes as customers’required
Product Packing