Chromite sand powder

Chromite sand powder is a product of south africa natural chromite ore after crushing and sieving. We import crushing Chrome ore from South Africa, wash, dry, dust cleaning, sieve and pack in China port, then export to all over the world directly, and its main chemical composition is Cr2O3. Chromite sand has good thermal conductivity, good resistance to thermal shock, excellent resistance to metal penetration or burn-on, resists slag attack and high dimensional stability.chromite sand powder is mainly used in glass production.

$330.00 – $550.00 / MT

Chromite sand powder available size:200mesh 325mesh 400mesh
Chromite sand specification is as follows:
Origin:south africa

ItemIndex
Cr2O3≥46.0%
SiO2≤1.0%
FeO≤26.5%
CaO≤0.30%
MgO≤10.0%
Al2O3≤15.5%
P≤0.003%
S≤0.003%
Cr/Fe1.55:1
Bulk Density2.5-3
ColorBlack
PH7-9
The amount of the acid≤ 2 ML
Percent soil≤0.1%
Percent Moisture≤0.1%
The sintered1600℃
Percentage of free acid present in the sand0
filling density 2.6g/cm³
sintering point> 1800°C
melting temperature 2180°C