chromite sand AFS45-50 south africa
chromite sand chemical-physical properties
| tem | Index |
| Cr2O3 | ≥46.0% |
| SiO2 | ≤1.0% |
| FeO | ≤26.5% |
| CaO | ≤0.30% |
| MgO | ≤10.0% |
| Al2O3 | ≤15.5% |
| P | ≤0.003% |
| S | ≤0.003% |
| Cr/Fe | 1.55:1 |
| Bulk Density | 2.5-3 |
| Color | Black |
| PH | 7-9 |
| The amount of the acid | ≤ 2 ML |
| Percent soil | ≤0.1% |
| Percent Moisture | ≤0.1% |
| The sintered | 1600℃ |
| Percentage of free acid present in the sand | 0 |
| filling density | 2.6g/cm³ |
| sintering point | > 1800°C |
| melting temperature | 2180°C |
Application:Foundry,refractory
Packing:1mt big bag