Chromite Flour: Core Raw Material for Magnesia Chrome Bricks, Key Powder for Spinel Phase Formation
Chromite flour is refined by crushing, grinding and screening high-grade South African chromite ore. It is the core raw material for manufacturing directly bonded magnesia chrome bricks, rebonded magnesia chrome bricks and sintered magnesia chrome bricks. It is also the key powder to form magnesium chromium spinel phase at high temperature.
The chromite spinel components in chromite flour undergo solid-state reaction with magnesia during high-temperature sintering and generate magnesium chromium spinel (MgCr₂O₄), forming a stable direct-bonded structure. This spinel phase features high temperature resistance, excellent alkaline slag corrosion resistance and low thermal expansion coefficient. It can greatly improve the refractoriness under load, hot strength, creep resistance and thermal shock stability of magnesia chrome bricks. It reduces cracking and spalling during intermittent furnace start-stop and extends the service life of refractory lining.
We strictly control impurities such as SiO₂ to avoid forming low-melting silicate phases which degrade refractory performance. The mainstream grade has Cr₂O₃ ≥44–46.0%. Common fineness includes 200 mesh and 325 mesh. It has uniform particle size, low moisture and low caking tendency, suitable for batching, mixing and firing processes of various magnesia chrome bricks.
✅ Main Applications Lining of AOD, VOD and RH vacuum refining furnaces; slag line of copper, nickel and other non-ferrous smelting converters and flash furnaces; high-temperature kilns such as cement kilns exposed to severe alkaline slag attack.
We supply imported refractory-grade South African chromite flour with stable specifications. Samples and COA test reports are available.
Physical & Chemical Properties of South African Chromite Flour
| Physical Properties | Chemical Composition | ||
|---|---|---|---|
| PH | 7–9 | Cr₂O₃ | 44–46.0% |
| Color | Bright black | SiO₂ | ≤1.0% |
| Acid Consumption | ≤2 ml | Fe₂O₃ | ≤26.5% |
| Mud Content | ≤0.1% | CaO | ≤0.30% |
| Bulk Density | 2.5–3.0 g/cm³ | MgO | ≤10.0% |
| True Density | 4.0–4.8 g/cm³ | Al₂O₃ | ≤15.5% |
| Moisture | ≤0.1% | P | ≤0.003% |
| Sintering Temperature | ≥1800℃ | S | ≤0.003% |
| Packing Density | 2.6 g/cm³ | Cr/Fe Ratio | 1.55:1 |
| Free Acid | 0 | ||
| Melting Point | ≥2180℃ |