Chromite Flour for Art Kiln-change Glaze | Low-Silicon Chromite Powder Imported from South Africa

Chromite Flour for Art Kiln-change Glaze | Low-Silicon Chromite Powder Imported from South Africa

South African low-silicon chromite flour is natural spinel chromite ore. It is refined by ore dressing, magnetic separation, ultra-fine grinding and classification. It is a preferred natural mineral colorant for art ceramic kiln-change glaze, crystal glaze and antique glaze. Different from synthetic chromium oxide green, its natural Cr-Fe coexisting structure delivers soft color gradient and good flow effect under high-temperature firing. Low silica design effectively reduces glaze defects such as pinholes, blisters and crawling. Stable Cr/Fe ratio guarantees consistent color from batch to batch.

Core Advantages

  • Strictly controlled SiO₂ ≤1.0%, fewer glaze surface defects
  • Cr₂O₃ ≥46%, stable Cr/Fe ratio, rich olive green, brown-green and tea tone for kiln-change effects
  • High thermal stability, suitable for oxidation and reduction firing in shuttle kiln, roller kiln and electric kiln
  • Low calcium, sulfur and phosphorus, less black speck pollution, compatible with multiple glaze systems
  • Cost-effective natural mineral pigment for art ceramics and antique tiles

Available Grades

200mesh, 325mesh, 400mesh, 600mesh, 800mesh, 1200mesh. Custom particle size and COA test report are available.

Chemical Specifications

Cr₂O₃ ≥46.0%,

SiO₂ ≤1.0%,

FeO ≤26.5%,

Al₂O₃ ≤15.5%,

MgO ≤10.0%,

CaO ≤0.30%,

S ≤0.003%,

P ≤0.003%

Appearance: Dark brown fine powder

True Specific Gravity: 4.0–4.6 g/cm³

Refractoriness: 1800℃

Applications

Art ceramic kiln-change glaze, crystal glaze, flow glaze, antique glaze, hand-made pottery glaze, tea ware glaze, decorative ceramic glaze.

Scroll to Top